Front Sandy (white)

Front Sandy (white)

FRONT

FINISHING PLASTER

FOR INDOOR AND OUTDOOR USE

  • High-quality alignment
  • High whiteness
  • Applied to a surface easily
  • Ideal for rooms with high humidity
  • Strong and plastic
  • Crack resistant
  • Weatherproof
  • Waterproof
  • Easy to use
  • Freeze proof
  • Layer thickness of 1-3 mm
  • Vapor permeable
  • High adhesion


Quality Certificate:
CE

EN 998-1:010

EN 998-1-GP-CSIII-W0

Dry building mix  ТМ MASTER  C.1.SHT1 white DSTU B V.2.7-126:2011

Bar-code: 4820086380263

25 kg +/-1%

Plastering mix ТМ MASTER. FRONT. No-fine White designed to prepare concrete, brick and plastered surfaces outside and inside buildings for various finishing and painting (thickness 3 mm); for window jamb extensions, surfaces for white and light finishing coatings. Effectively used in areas with high humidity (kitchens, bathrooms).   

SURFACE PREPARATION

Surface preparation must be done in accordance with the State Building Standard of Ukraine DBN V.2.6-22-2001. The base must be:

- clean (remove dirt, flows, dust, fungal lesions with a power tool or manually);

- strong (not lower than the coating strength);

- in presence of cracks (to be grouted), drops or irregularities treat the base with ТМ MASTER, and then align with the mineral mix for plastering, for example ТМ MASTER. FRONT. Sandy White (72 hours before the start of work);

- to enhance adhesion and reduce water absorption, prime the surface 4 hours before plastering using the primerТМ MASTER;

- glassy surfaces must be made rough;

 

WORK PROCEDURE

Perform the work at air and surface base temperature of+50С to +250С. During the work eliminate the possibility of precipitation.

Two days before the start of plastering, in the process of its performance, and for three days after the end, maintain the temperature not below +50С and not above +250С. Add pure water to the dry mixture in an amount indicated in specifications, then mix it (use electric drills with screw socket). Leave closed mix for 5 minutes, then stir again. The closed mix is suitable for use for 120 minutes (under recommended atmospheric conditions). Apply the closed mix ТМ MASTER. FRONT. No-fine White on the surface with a uniform layer with a thickness of 3 mm using a trowel or a float. Conduct plastering continuously following the wet-on-wet jointing rule.

The applied layer must be evened before the beginning of the closed mix solidification. Float the surface of the finishing mix TM MASTER. FRONT. No-fine White, and apply the finishing coating no earlier than 72 hours after application of the mix.


NOTE TO A BUYER

- The base strength must be not less than the strength of the mix;

- Failure to follow the instructions for use mentioned on the package may adversely affect the aesthetic and performance properties;

- Products are not subject to mandatory certification;

- The mix is safe for human health in the production, transportation, storage, application and during the operation subject to following the requirements of this standard to production safety and health;

- Keep away from children;

- Date of manufacture, shelf life and batch number are mentioned on the package;

- Use only for the intended purpose.

- The manufacturer is not responsible for the use of the material for the purpose and under conditions not covered by this instruction.

- This instruction is a recommendation and does not substitute the professional training of the contractor.          

 Dry building mix  ТМ MASTER  C.1.SHT1 white DSTU B V.2.7-126:2011

Ingredients

 

Cement mix modified by mineral fillers and polymeric additives

 

Size of aggregate

 

maximum 0.8 mm

Time the mix is suitable for use

 

120 minutes

Open time

20 minutes

Strength of adhesion to base

0.3 MPa

Max compressive strength

7 MPa

Recommended amount of water for preparing the mix

0.35 L / 1 kg of dry mix

Температура использования

от +5°С до +30°С

Consumption

1.1 kg / m2 / 1 mm

All of these recommendations are efficient at +20С and relative humidity of 60%.

 

SAFETY RULES

 

Dry building mixture contains cement, which causes alkaline reaction in hydration. When using the mix, use the personal protective equipment (respirator and rubber gloves). When working, protect the skin and eyes. In case of a mixture contact with eyes, rinse them immediately with plenty of water and seek medical advice.

 

Expiration date: 6 months from the date of manufacture mentioned on the package.

 

Must be disposed of in accordance the State Standard of Ukraine DSanPiN 2.2.7.029

 

Storage conditions: Store in the original intact packaging, on pallets, in dry premises at temperatures below 400С and humidity of 75%.

 

Warranty period: The manufacturer guarantees compliance of the quality with the requirements of this standard for the period specified on the package, provided the requirements of transport and storage are followed.